Easy-to-clean

SCHOTT AO Pikto Clean 640x390px
In addition, an Easy-to-Clean functionality can be optionally combined with LUXADUR™.

This enhancement adds an additional layer to the scratch resistant anti-reflective coating and eases the cleaning of the watch’s glass. Fingerprints, dirt or other contaminations can be cleaned by a simple swipe with ease.

SCHOTT utilized its decades of experience in Easy-to-Clean and Anti-Fingerprint coatings to develop a unique product perfectly adapted for the watch industry in respect to cleanability, durability and anti-fingerprint properties.

SCHOTT developed a unique test to ensure excellent anti-fingerprint properties utilizing artificial fingerprints and stray light evaluation. Less stray light signifies reduced visibility of fingerprints retaining the pristine impression of the watch dial.